Abasse Kamarchou، S. Atia، Ammar Zobeidi، H. Chettah، Laboratoire d’énergétique et d’électrochimie du solide, Département de génie des procédés, Faculté de Technologie, U. F. A. Sétif 1, Sétif, 19000, Alegria✉، S. Benhamida، Univ. Ouargla, Fac. des Mathématiques et des Sciences de la Matière, Lab. Rayonnement et Plasmas et Physique de Surface, Ouargla 30 000, Algeria، D. Abdi، Laboratoire d’énergétique et d’électrochimie du solide, Département de génie des procédés, Faculté de Technologie, U. F. A. Sétif 1, Sétif, 19000, Alegria، F. Rahal، Laboratoire d’énergétique et d’électrochimie du solide, Département de génie des procédés, Faculté de Technologie, U. F. A. Sétif 1, Sétif, 19000, Alegria، A. Berchi، Laboratoire d’énergétique et d’électrochimie du solide, Département de génie des procédés, Faculté de Technologie, U. F. A. Sétif 1, Sétif, 19000, Alegria، Nacer Chaabia، Laboratoire d’énergétique et d’électrochimie du solide, Département de génie des procédés, Faculté de Technologie, U. F. A. Sétif 1, Sétif, 19000, Alegria

الملخّص

"Effect of zinc salt concentration on the growth of electrodeposited zinc oxide phases was investigated. ZnO thin films were elaborated via chronoamperometry on fluorine doped tin oxide (FTO) substrates from aqueous mixed bath of zinc nitrate and chlorate at 70°C. X ray diffraction patterns showed nanocrystalline films of hexagonal wurtzite phase with (101) preferential orientation for ZnO as grown in low concentration of Zn2+ salt. High concentration of Zn2+ favor the formation of Zn5(OH)8Cl2H2O simonkolleite phase. After heat treatment at 400 °C for 1h this later decomposes to ZnO oxide which presents no preferential orientation. The route mean square RMS roughness of surfaces estimated from AFM technique shows that ZnO generated from heat treated Zn5(OH)8Cl2H2O present more increasing roughness than ZnO deposits obtained at lower salt concentration. The photoelectrochemical answer indicated important generated photocurrents for both films which present n-type electrical conductivity"

التفاصيل

اللغة الأصليةEnglish
المجلّةChalcogenide Letters
المجلّد19
العدد7
الصفحات447-456
ISSN1584-8663 · 1841-4834
DOI10.15251/cl.2022.197.447
حالة النشرمنشور — 1 جوان 2022

الكلمات المفتاحية

البصمة